The nanostructure of each surfactant treated catalysts was slightly agglomerated from original pattern after subsequent thermal treatment at 400 C (Fig. 5c1–e1).
The nanostructure of each surfactant treated catalystswas slightly agglomerated from original pattern after subsequentthermal treatment at 400 C (Fig. 5c1–e1).