Gate location has a major impact on the amount of initial molecular orientation that
exists across the hinge. Mold cavities must be filled perpendicular to the hinge plane so
that once the melt front hits the hinge, it will continue flowing across without interruption
until volumetric fill is reached. The gate(s) should be positioned so as to prevent weld
line formation and/or air entrapment along the hinge area.