Materials
The experimental was started with the procurement of the Komeng coconut shell, epoxy resin, hardener, SRM mould and PP. The coconut shell was collected from the coconut farm district of Manjung Perak MalaysiaThe resin used was epoxy resin 3554A with the density of 1.15 g/cm3. The SRM open mould type was used with rectangular shape according standard (ASTM D256) for Izod impact test and dumbbell-shape samples follow the standard ASTM D2099 for tensile test.