The experiment was carried out with a DMTA Rheometricsscientific strain control at a frequency of 1 Hz with deformationamplitude of 0.1% to insure experimentation in the linear viscoelas-ticity region. The heating rate was 3◦C/min from −100◦C to 100◦C.