preparation of catalyst by dry impregnation after support Calcinations at temperature 550 2 hr to get rid of the impurities mixed in a solution of sodium carbonate 45% dryer at temperature 120 16 hr Calcinations temperature 550 5 hr the catalyst received to keep it in Disiccator before test reaction