The mixing for each batch took 10 min: PP was first added into the mixing chamber and mixed for 1 min; then the stabilizers were fed to the molten PP and 1 min later NR was added to the mixer; after another 3 min of mixing the peroxide was added and the mixing continued for another 5 min to complete the dynamic vulcanization process.