The adhesives were cured in an oven at 120 72° C until a constant weight was obtained and ground into a powder. XRD patterns were recorded on an XRD diffractometer (XRD-6000, Shimadzu, Kyoto, Japan ) using a cobalt source and 0.2 theta scan ranging from 5° to 80° at 45 kV and 30 mA.