1 kg crushed clean ore sample was ground in a laboratory stainless
steel rod mill with stainless steel rods at 50% solids to obtain
80% particles passing 212 lm with the addition of 8 g/t Cytec
3894A. The mill discharge was then transferred to a 3.0 L Agitair
flotation cell.