Measuring the antistatic performance by the surface resistivity meter. You can
check whether it satisfies the reference value for each coating more than 1
minutes after the application. For example, the resistance value at the surface
of the substrate was measured from 11 to 12 square of 10 prior to the
application, however it was measured from 8 to 9 square of 10 after the
application.