For a typical procedure, 10 g F127 copolymer was mixed with 85 g ethanol. The resulting solution was heated up to 40 C to
form a clear solution under stirring. 25 g resol alcoholic solution (40 wt%) was added in the above solution and kept stirring
at room temperature over 6 h to obtain the precursor solution