In all cases, the final residue after
TGA is approximately 30% of the weight. This result indicates
that each blend forms a similar residue irrespective of the
PANI content. The PANI-DBSA salts were not completely
destroyed, because in nitrogen atmosphere, carbonisation of
polymer takes place leaving a marked residue.