1) As before, prepare the blocks for wringing.
2) Wipe the surface of the Optical Flat gently across the oiled Wring Pad.
3) Wipe the surface of the flat gently across the dry pad.
4) Slide the test block onto the flat as shown. Apply pressure while sliding the block and flat together.
5) Observe the surface of the gage block that is wrung to the Optical Flat from the opposite side of the flat. Repeat this step as necessary to ensure a valid result.
6) Interpret results:
a) For Federal Grades 0.5, 1, and 2, and ISO Grades K, 00, and 0, no color or oil should appear on the face of the flat.
b) For Federal Grade 3 or ISO Grades 1 and 2, the surface shall not have less than 80% colorless wringing area.
7) Repeat for the other surface of the test block.
This test (at right) may be difficult to apply to gage blocks that are not almost perfectly flat. This includes thinner gage blocks that are less than .100” or 2.5 mm thick, which are not usually, flat in their free state. This includes most gage blocks in metric sets.
1 ) ก่อนเตรียมบล็อกสำหรับจับ .
2 ) เช็ดพื้นผิวของแสงแบนค่อยๆผ่านน้ำมัน เอาแผ่น
3 ) เช็ดผิวเบา ๆทั่วแผ่นเรียบแห้ง
4 ) เลื่อนการทดสอบบล็อกบนแบน ดังรูป ใช้แรงดันในขณะที่เลื่อนบล๊อคและแบนกัน
5 ) สังเกตผิวของเกจบล็อกที่ถูกบีบให้แบน แสงจากด้านตรงข้ามของแบน ทำซ้ำขั้นตอนนี้เท่าที่จำเป็นเพื่อให้แน่ใจว่าผลที่ถูกต้อง
6 ) ตีความผลลัพธ์ :
) สหพันธ์เกรด 0.5 , 1 , 2 , และ ISO เกรด K , 00 , 0 , ไม่มีสีหรือน้ำมันควรจะปรากฏขึ้นบนใบหน้าของแบน
b ) Federal เกรด 3 หรือ ISO เกรด 1 และ 2พื้นผิวจะไม่น้อยกว่าร้อยละ 80 ไม่มีสี จับพื้นที่
7 ) ทำซ้ำสำหรับพื้นผิวอื่น ๆของการทดสอบบล็อก
ทดสอบนี้ ( ขวา ) อาจจะยากที่จะใช้กับเกจบล็อกที่ไม่ได้เกือบจะสมบูรณ์แบบแบน ซึ่งรวมถึง ทินเนอร์ เกจบล็อก ที่น้อยกว่า 100 " หรือ หนา 2.5 มิลลิเมตร ซึ่งมักจะไม่แบนในรัฐอิสระของพวกเขา นี้รวมถึงบล็อกเกจมากที่สุดในชุดตัวชี้วัด
การแปล กรุณารอสักครู่..