Petrothene LR 734001 (melt index 0.38 dg/min, density 0.954 g/cm3), an HDPE from Equistar Chemicals, was used as the polymeric matrix. Commercial wood flour from hardwood maple was used as the filler. This wood flour was low specific gravity (0.54), standard grade (100-mesh size) supplied by American Wood Fibers. Three endothermic CFAs [BIH40, sodium bicarbonate (SB), and FP] and three exothermic CFAs (Celogen-OT, Celogen-AZNP, and EX210) were utilized in this study. The detailed information on all these CFAs is described in Table I. Among the CFAs used, BIH40 and EX210 had polymer carriers, whereas SB, FP, Celogen-OT, and Celogen-AZNP had no polymer carrier. Maleated PE with a melt flow rate of 5 dg/min and a percentage of functionality of 1.0 (Polybond 3009, Uniroyal Chemicals) was used as the coupling agent.
Petrothene LR 734001 (ละลายดัชนี 0.38 dg นาที ความหนาแน่น 0.954 g/cm3), HDPE จาก Equistar สารเคมี การใช้เป็นเมตริกซ์เมอร์ ค้าไม้ flour จากไม้เมเปิ้ลถูกใช้เป็น filler flour ไม้นี้ถูกแรงโน้มถ่วงต่ำ specific (0.54), เกรดมาตรฐาน (ขนาด 100-ตาข่าย) มาจากเส้นใยไม้อเมริกัน สามดูด CFAs [BIH40 โซเดียมไบคาร์บอเนต (SB), และ FP] และสาม CFAs คายความร้อน (Celogen-OT, Celogen AZNP และ EX210) ถูกใช้ในการศึกษานี้ ข้อมูลรายละเอียดเกี่ยวกับ CFAs เหล่านี้อธิบายไว้ในตารางผม ระหว่าง CFAs ใช้ BIH40 และ EX210 ได้พอลิเมอร์สายการบิน ในขณะที่ SB, FP, Celogen OT และ Celogen-AZNP มีผู้ขนส่งไม่พอลิเมอร์ PE maleated ละลายตัดค่าเสื่อมราคา 5 dg นาทีและเปอร์เซ็นต์ของ 1.0 (Polybond 3009 เคมี Uniroyal) ถูกใช้เป็นตัวเชื่อมต่อแทน
การแปล กรุณารอสักครู่..