The as-grown single crystals were ground and put in a capillary
of 0.3 mm diameter for powder X-ray diffraction (XRD) measurement.
The XRD patterns were collected on a Stoe Stadi-P diffractometer
with Cu kα radiation (λ¼1.5406 Å), using Debye–Scherrer
mode.