It is imperative to note that the 28 days mean compressive strength of concrete specimens developed with 5–15% GRP waste powder using 2% superplasticiser resulted 70.25 ± 1.43–65.21 ± 0.6 N/mm2 which is about 45% higher than that of without the addition of superplasticiser (with GRP waste) and about 11% higher than that of the control concrete (without GRP waste) with 2% superplasticiser.