Generally it can be said that a
milling time of up to 60min is sufficient to obtain a homogenously
mixed sample that generates H2 with high intensity at temperatures
around 450 ◦C.However, prolonged milling time up to 120 min
results in a shift of H2 peak to over 500 ◦C and also decrease in
intensity.