It is also seen that a crack running through the wood flours, and this could be an indication of stress-transfer
from the matrix to the wood flours. The interfacial bonding between the filler and the PP matrix is improved
due to the esterification mechanism and the fracture occurred at the filler itself. This means that the stress is