The hydrogen crossover, determined with linear sweep voltammetry,
was found to be below 1 mA cm2 for all cells and did
not change significantly after the 94 h OCV hold testing. The ECA of
the catalyst was found to be around 65 cm2 Pt gPt1 and decreased
during testing for all cells