the degreased steel samples were always electroreduced (i//1.0 mA/cm2) for 20 min in an aqueous 1.0 mol/l HNO3 solution. The pretreated sample was then immersed in the electrolytic solution (5 mol/l H2SO4/2.5 mol/l CrO3) and immediately submitted to an alternating potential pulse