Data obtained by this test method may supplement that from test method D1004, wherein the specimen is strained at a rate of 50mm [2 in] per minute However specimen geometry and testing speed of the two test method are dissimilar. The rate of tearing in this test method, while varying as a function of resistance to tear is in The range from 7.6 to 46 m [300to 1800 in.]/min