As compared with UH, the diffraction peak intensities of the calcined samples increase, indicating the improvement of crystallinity of anatase phase after calcination. The crystal sizes of UH, UH-350 and UH-450 determined by the Scherrer formula [11] from anatase (1 0 1) peak are about 6.2, 9.1 and 11.2 nm, respectively.