The demonstration of physical and mechanical requirements was specified by demonstration of compressive
strength using cubes as test specimens. The value of compressive strength ranged around 1 MPa in all SPs after 28
days curing. The decrease of the strength over time may be caused by the chemical reaction between unreacted
components of the NS and the matrix causing gradual degradation of the SPs.