The bands relative to cellulose were more intense in the spectra
of the treated samples, because lignin removal augmented their
crystalline content. Indeed, the peaks assigned to the cellulose CeH
groups stretching in the 1400e1300 cm1 region were more
intense in the treated samples as compared with the bran.