The ball-on-disc tribo-testing system (CSM Instruments, Co., Ltd.) was employed to measure the transient of friction coefficient under high pressure condition. SUJ2-ball with the diameter of 6 mm was used as a counter material. The applied load was constant, 10 N, and, the sliding velocity, 150 mm/s.