The flow rate of argon was kept constant at 100 ml/min. To purify the obtained products, oxidation in air at 470 ◦C was carried out for 20 min at a fast heating rate (10 ◦C/min), followed by acid etching using 45 wt% HF for 24 h and a 10 wt% HCl solution to remove the zeolite support.