A clean with a solution of diluted potassium silicate (200 mL in 10 L)
just after saw damage etch and texturing. The solution is agitated for 3 minutes and
wafers are immersed in it for 7 minutes. Followed by cleans in RCA-B solution, Piranha
solution and BOE solution.