For its conversion into tellurium oxide, the precipitated elemental tellurium was weighed into a porcelain crucible, heated successively at 100 ◦C for 30 min, at 300 ◦C for 1 h, and at 600 ◦C for 1 h in air,then cooled in a silica gel desiccator for 1 h, and weighed.