Therefore, the hemicelluloses are much more easily degraded with respect to acid catalysed hydrolysis. Due to the structure of these polysaccharides, the furans, especially in more acidic oils. Might very well be significantly produced from the hemicelluloses due to a chemical degradation. This would then mean that the concentration of the furans cannot directly be coupled to the DP of the insulation paper.