Increasing
the PEO loadings (20–40 phr) rendered higher absorbency with lower mechanical strength.
A higher scorch time and cure time with a lower crosslinking density and cure rate index
were found in the MNR-modified WSNRs compared with the unmodified WSNR or ENRmodified
WSNR.