Composite samples comprising Fe-based metallic glass particle and the crystalline Ni matrix were produced. Were behavior was investigated by a pin-on-disc type tester using hardened steel as the counter material. It was concluded that the wear mechanism depended on the volume fraction of crystalline nickel in the composites. The transition from the brittle fracture to the adhesive wear was observed by increasing the volume fraction of ductile Ni in the composites.