1. We’ll make PVD-TiCN coating again in NISSIN.
2. If this die life is very short comparison to normal using, we’ll
re-make it.
3. From next time, we’ll change the coating maker to UTT.
But I’m afraid it’ll take another about 2 or 3 days more than current
NISSIN.
The color of UTT seems to be dark violet + gold color.