To study the effects of Cl− on SCC behavior at different temperatures, crack growth rate measurements at the same water
chemistry conditions were repeated at temperature of 288 ◦C. The crack growth rate at 288 ◦C was established and stabilized at 2.56 × 10−8 mm/s under HWC conditions which is about 2 times lower than at 325 ◦C.