Figure shows the fatigue data which indicates the reduction
of allowable fatigue stress as the number of cycles increases,
86.2 N/mm2is the fatigue limit corresponding to one million
or 10 lakh cycles. The alternating stress induced in the fatigue
analysis is 62 N/mm2 which is less than the allowable
fatigue limit stress of 86.2 N/mm2. So structure is safe for the
fatigue design. Stresses are captured for maximum stressed
node 200327 on the cam lobe.