We want to request shinko reduce step of produce lead frame and still maintain the quality.
Shinko reply to can't reduce process because them AG side bleed out capability is (X2 of material thickness from mask line)
Therefore if them apply normal Ag process, the position of Ag side bleed out will be 2.425-2.725 mm from center line.
Therefore, them have apply for this parts.