Lignite from the Thar Coal Mine, Sindh Province,
Pakistan, were ground and passed through a 60-mm
sieve, and then treated with an oxidizing agent (100
mL L−1 HNO3) added in small doses at specific intervals
to prevent rise in temperature to above 40 ◦C due
to exothermic oxidation with external cooling in laboratory