Our
results demonstrate that exclusive stereocomplex crystallites
without homocrystallites of high-molecular-weight PLA can be
formed at processing temperature as low as 160 C, either at
equimolar PLLA/PDLA blends or non-equimolar PLLA/PDLA (60:40)
blends.