It is well known the addition of organic residues produces an increasing of porosity in ceramic bodies since the organic matter is burning during the firing process [49].
SMC added increases the AP from 27.5% (without SMC) to 33% (with 17% of SMC added).
These results were found similar than those reported by literature where AP ranges from 32% to 39%