Designing a new glaze system having higher scratch resistance
requires more silica to be present in glaze formulations.
However, because of low TEC of silica (0.54×10−6 ◦C−1),
the overall TEC value of glazes would be reduced. This would
create a TEC mismatch problem with commercial bone china
body.