The extraction treatment which bagasse receives prior to bulk storage has a
significant influence on subsequent spontaneous combustion behaviour.
Upstream of the final mill bagasse is saturated with high temperature water (80-90 °C). Final bagasse leaves the milling train by open conveyor at a temperature
of 55-65 °C. “Then bagasse is loaded into storage piles, the temperature has decreased slightly to 48-60 °C and the pl-I lies in the range 5.5-6.7’. '