the presence of a sharp and strong non-polar optical phonon E2H mode at 438 cm− 1 confirms that the products formed are wurtzite hexagonal ZnO.
Two very small peaks at 332 and 376 cm− 1 were also obtained which were assigned as E2H–E2L (multi-phonon)
and A1T modes, respectively [12].