Characteristic features
Irregular, small to large-area solid metallic thickening, frequently several millimetres thick. Such defects often run parallel to the casting surface, their own surfaces being rough. The edges frequently exhibit so-called “undercuts”. Castings with solid scab-bing often exhibit sand crust inclusions