This involves a more cohesive microstructure with an overlap of 14.0% compared to samples prepared with printing width set at 200 and 300%. Indeed, these latter samples do not undergo any overlap (along the entire sample length),
This involves a more cohesivemicrostructure with an overlap of 14.0% compared to samplesprepared with printing width set at 200 and 300%. Indeed, these lattersamples do not undergo any overlap (along the entire sample length),