Therefore, even the mortar with higher replacement ratio of NS
with BBA (20% by volume) and 450 g of CEM-II, i.e. the one with the
lower mechanical characteristics, can be applied as bedding mortar
in walls and other building elements, complying with a minimum
of 2500 psi (17.23 MPa) of compressive strength (according to
ASTM C 270).