Results showed that the highest liquefaction percentage was 99.79% under the optimal conditions
(liquid–solid ratio 6:1; temperature 150 C; reaction time 80 min; raw size more than 40 mesh; catalyst
mass percentage of solvent 4%; solvent volume ratio 3:1). Polyols could be obtained effectively by the liquefaction
of BSS, an agricultural by-product.