Table 1, Table 2 show the physical andmechanical
properties of natural wood and treated wood.All of
themechanical properties of the treated woodwere
improved compared to the natural wood. The basic
density of polar wood increased from 0.214 g/cm3
to 0.268 g/cm3 fromthe Table 1; and the dimensional
stability was also improved as shown in Table 2.