During the process, the conversion of pumice powder into
silica reaches a rate of 94%. This constitutes an important
and efficient method for preparing nanosilica with mesoporosity
(a pore distribution of 2–6 nm) and a large surface
area (422 m2/g), which can be easily produced on a large
scale.