fabrication with the Hþ-form membranes. Decal electrodes sandwiching Hþ-form membranes were hot-pressed at five different temperatures ranging from 140 to 180 C to prepare MEAs. Pressure was maintained at 3.0 MPa with a fixed roller speed of 50 mm min1.