Here, the 1 wt% of the loss at 100–200 C is contributed
by loss of absorbed water from FRBM and the sharply weight loss
of 2.5 wt% at 350–430 C is ascribed to thermal decomposition of
brucite [19] which coincides with the main degradation temperature
350–380 C for PP