(Fig. 6), a sharp band appeared at 3600 cm1 for
both of the preserved catalysts (Fig. 6b and c) whereas no such
peak was observed in the spectrum of the fresh catalyst (Fig. 6a).
This peak can be assigned to the OH group bonded to the catalyst,
caused by moisture during the storage