Here, DHsample is the area under the curve between 65
and 160 C and DH0m
is the enthalpy of melting for a fully
crystallized PLLA sample (93.1 J$g1 [14,21]). The calculation
reveals that the crystallinity of the PLLA fibers is
essentially unchanged during the degradation, even for the
highest degradation time (Fig. 5).